【摘 要】
:
A 92WC-8Co powder mixture with 33 nm WC grains was prepared by strengthening ball milling and was then sintered by spark plasma sintering (SPS) at 1000- 1200℃
【机 构】
:
School of Materials Science and Engineering, Shanghai University, Shanghai 200072, China;Materials E