论文部分内容阅读
本文概述了可锻铸铁热浸镀铝石墨化这项新工艺的探索性试验。低碳可锻铸铁在760~780℃纯铝浸镀液中,只需浸镀五分钟,即可完成热浸镀铝石墨化过程,并试验分析了生产低碳珠光体基体可锻铸铁铁帽的可能性。
This article provides an overview of the exploratory testing of this new process for malleable cast iron hot-dip aluminide graphitization. Low-carbon malleable iron In 760 ~ 780 ℃ pure aluminum immersion bath, immersion only five minutes to complete the process of hot-dip aluminide graphitization, and experimental analysis of the production of low-carbon pearl matrix malleable iron iron cap possibilities.