论文部分内容阅读
在同时处理霞石和高岭土生产氧化鋁时,为了提高氧化鋁的提取率和减少試剂的用量,事先用含150~170克/升Na_2O的循环碱液在90~95℃下,对高岭土进行处理。
In order to increase the extraction rate of alumina and reduce the amount of reagents when alumina is processed simultaneously with nepheline and kaolin, kaolin is previously treated with a circulating alkali solution containing 150 to 170 g / L of Na 2 O at 90 to 95 ° C .