大型双钼丝环孔型线切割机床

来源 :上海金属.有色分册 | 被引量 : 0次 | 上传用户:leolee4510
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
“双钼丝环孔型线切割机床”研究项目已于1986年10月30日在市科委主持下通过了专家鉴定验收。该项目由上海第一铜管厂等单位共同完成。这台机床主要加工轧辊的孔型空间曲面,用普通机械加工很难完成,即使完成了还有热处理变形问题。它可在x、y轴移动和z轴旋转,采用了双丝架,双钼丝同时切割,既可提高生产效率,又能保证加工轧辊的质量,若装配专用夹具后,就能加工双线轧机的轧辊,每次可加工四根(一 “Double molybdenum ring hole cutting machine tool” research project was October 30, 1986 under the auspices of the Municipal Science and Technology Commission passed the expert appraisal. The project by the Shanghai First Copper Tube Factory and other units to complete. This machine tool main processing roller hole space surface, with ordinary machining is difficult to complete, even if there are still heat treatment deformation. It can move in the x, y-axis and z-axis rotation, using a double wire frame, double molybdenum wire cutting at the same time, both to improve production efficiency, but also to ensure the quality of processing roller, if the assembly of special fixture, you can process double line Rolling mill, each can be processed four (one
其他文献
我厂是空军后勤的企业化军办工厂,1986年被总后勤部任命为中国人民解放军九五五二工厂,位于武汉东湖之滨,是机械委数显表定点生产厂。技术力量雄厚,设计生产SF系列数显表已
我国可锻铸铁的产量相当长一段时间都排回在年产30万吨的水平上,直到近两年才有了相当大的发展,一跃而为年产45万吨,成为我国第二大铸铁产品(仅次于灰铸铁)。而且已成为我国
一、指甲盖状缺陷的产生图1为我厂采用金属型浇注的气缸盖铸件,其材质是ZQAL9-2,铸件耍求经机加工后,在气压为225kgf/cm2状态下,保压5 min不得泄漏。在设计铸造工艺时,金属
某型导弹弹体大型模胎的材料结构历经硬木、铸铝、环氧塑料及铸铝填敷环氧塑料四次改革。在铸铝模胎上分区段填敷环氧塑料较之浇注法有更多的优越性。填敷法操作方便、节省原
这种工具(图1)能清除钻孔(φ24)后传动轴叉斜面上的毛刺。它由刀杆1及装在刀杆槽内并固定在轴3上的清理刀片4组成。刀杆座内有一弹簧5,能产生清除毛刺所必需的力,并使刀片恒
我厂在研制高精度的球面车床中,上、下回转盘的多环导轨的加工质量直接影响球体的加工精度。多环导轨如图1所示。上、下回转盘各有4条环形导轨,V型槽的夹角为90°,槽的最大
本文研究了功率密度为(1—1.4)×10~4W/Cm~2激光束对几种常用工具钢T10A、9CrSi、GCr15、CrWMn、W18Cr 4V进行扫描后,表面强化层组织、硬度分布。结果表明激光处理表层硬度比
我们知道,深拉延件首次拉延后的各次拉延,大致有两种方法,一种是正拉延,另一种是反拉延。近年来,我们对原来采用正拉延的筒形件,改用反拉延的方法,收到了较好的效果。一、提
在铸造生产中,经常会碰到一些大中型圆筒类铸件,外部分布着几道环状加强筋,与数条直筋呈十字形交叉连接(如图1)。这类铸件,对于某些厂家,在没有专用砂箱,无法进行多箱造型的
我们用T10A钢冷拔线材制造小型丝锥,在淬火时竟出现成批的纵向裂纹。经分析,开裂产生的主要原因是丝锥淬火前残余应力过大。我们在淬火之前,将丝锥进行正火,即在800℃的盐浴