防止石棉水泥瓦裂纹的办法

来源 :建筑材料工业 | 被引量 : 0次 | 上传用户:lovegyyf
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
石棉水泥瓦产生裂纹的原因主要有以下几方面: 一、原料1.石棉含砂石、粉尘多,吸附水泥的性能低,瓦硬化后结构松弛、变脆,故容易发生断裂。2.如用角闪石棉制瓦,由于角闪石棉靱性低、脆性大、不易松解,也会发生裂纹。3.用矿渣或页岩水泥制造石棉水泥瓦,含水较多,水分蒸发后易产生干缩,稍加碰击便产生裂纹。4.由于玻璃丝纖维很脆、表面光滑,如加入量过多(12%以上——占石棉百分数)、瓦 Asbestos cement tile cracks mainly due to the following aspects: First, the raw material 1. Asbestos contains sand, dust and more, the performance of the adsorption of cement is low, the tile after hardening structure is loose, brittle, it is prone to fracture. 2. If tiles are made of amphibolite, cracks may also occur because amphiboles are low malleability, brittle, and difficult to release. 3. The use of slag or shale cement to produce asbestos cement tiles, containing more water, moisture evaporation easily produce shrinkage, a little hit will produce cracks. 4. Due to the brittle and smooth surface of the glass fiber, such as excessive addition (12% - asbestos percentage), watts
其他文献
沈阳市第一红砖厂隧道式干燥室投入生产后,经过不断改进,干燥周期已从初期的60小时缩短为40小时,合格率达到80~95%,最终含水率达到3~5%以下。一、改善热源供应,稳定热工制度今
住宅建筑物的朝向问题,在住宅卫生上是很重要的。由于住宅朝向不同,影响室内的微小气候,自然照明和紫外线量。紫外线量是一种对人体有积极作用的因素,长期不受紫外线照射或
企业文化作为一种特定社会组织的文化,是企业核心价值和经营理念等方面的体现,必然有其独特性。虽然不同的企业在企业文化理念的表达上千差万别,但是,作为社会独特组织的企业
1.调整 (1)深浅的调节。深浅调节主要靠拖拉机的悬挂系统来进行,调节悬挂系统的中央拉杆,当中央拉杆缩短,犁铲入土角增大,深度就增加;反之,中央拉杆伸长,入土角减小,深度亦
在机动化的战争中,布置和清整战地的模规和范围很大,因此对未来的战地工程机械提出了很多要求。为了增强我军的机动能力和限致敌军的机动能力,必须迅速修筑公路、清除障碍、
为研究由冷弯卷边H形开孔薄壁钢梁和预制轻骨料混凝土板形成的装配式组合楼板的受火性能,对6个两端简支组合楼板试件开展了高温下试验研究,得到了试件的温度及位移响应.研究结果表明:在等效均布荷载2.0kN/m2及最高炉温为600℃的烃类火灾作用下,以轻骨料混凝土及腹板开孔薄壁钢梁形成装配式组合楼板具有良好的抗火性能,组合楼板的跨中挠度最大为L/44(L为组合楼板跨度)时,试件仍保持良好的整体性;主钢梁腹
实创股份提出在继续加快科技园区开发建设的同时,着力完善自然、人文、科技创新“三位一体”生态体系,为科技企业和科技人员提供更好的创新创业环境和人居环境,努力将CID建成
广东省水泥制品厂試制成功一种套接式的輕型鋼筋混凝土电杆。这种电杆系由上下两杆組装而成,上杆外径86mm,壁厚20mm,长3.5m;下杆外径150mm,壁厚30mm,长1.5m。套接后电杆总长
驱动水泥窑、磨机、烘干机、输送机等设备的大中小型封闭式减速器中的齿轮,有的是标准切削制造,有的是特殊制造。修配时怎样区别齿轮啮合性质是标准齿轮,还是特殊齿轮呢?这
基于2 616 h的风场实测脉动风速数据,研究了风场的水平向风速空间相关函数,提出了湍流尺度内的相关函数模型。结果表明:空间相关性的强弱与风向角、空间间距和平均风速密切相