论文部分内容阅读
美国一家钢铁公司采用了一种薄板坯连铸与薄带钢轧制连续进行一次完成的新工艺。薄板坯连铸新工艺与传统的连铸工艺相似,不同之处在于前者板坯厚度为50mm,后者为200~250mm。钢的冶炼在电弧炉中进行。当废钢全熔后将钢液倒入容量为125吨的钢包内,然后把钢包移至铜包冶金站,
A steel company in the United States used a new process that was completed once in a row by thin slab continuous casting and strip rolling. The new process of thin slab continuous casting is similar to the traditional continuous casting process except that the former has a slab thickness of 50mm and the latter of 200-250mm. Steel smelting in the electric arc furnace. When the scrap after the molten steel poured into the capacity of 125 tons of ladle, and then moved to the ladle copper metallurgy station,