这里介绍的是在壁厚1.1毫米的附件上电解加工八个槽的问题。零件如图1所示。该零件原用机械加工制造,需先钻定位孔再铣槽。铣槽后大量毛刺留在槽子下部并往内翻,要花费大量时间和劳动力打毛刺。机加单件工时定额为65分钟。现采用电解加工一次成型,不到10分钟即可同时加工好6个零件,效率提高十倍。采用此种方法无需专用电解加工机床,一般的电解设备均能满足要求,只需根据所加工的零件制作一个简单的电解夹具,采用固定式 Here is the problem of electrolytically machining eight slots on a 1.1 mm wall thickness attachment. Parts shown in Figure 1. The parts were originally machined to be machined, drilling holes need to be drilled first and then groove milling. After milling slot a large number of burrs to stay in the lower part of the tank and turn inward, to spend a lot of time and labor burr. Machine plus a single working hours fixed at 65 minutes. Electrolytic processing is a molding, less than 10 minutes can be processed at the same time six parts, the efficiency increased tenfold. This method requires no special electrolytic processing machine, the general electrolysis equipment to meet the requirements, just according to the parts manufactured by a simple electrolytic fixture, the use of fixed
其他文献
本文扼要介绍国内一些单位对于锌,镉镀层有机气氛腐蚀的研究结果:对有机材料挥发的腐蚀性气氛和镀层腐蚀产物的主要成份进行了测试;初步探讨了气氛腐蚀的有关机理;研究了气氛
从对国外研究电泳涂漆方法的主要公司的专利的研究和分析中,可得出两个重要的最有前途的发展方向及其在工业中的应用方向:一、研究以新型成膜物质为基础的涂料及改进涂漆工
吹砂所用的喷砂咀,过去一直沿用苏联最落后的铸铁咀,使用寿命一般仅1~2小时就须更换,消耗量很大。有的工厂也陆续采用过陶瓷喷咀,寿命可达十几小时,有的采用硬质合金材料的喷
克鲁索-罗华公司发展了一种制造蒸汽发生器封头的新方法。这种方法的特点主要是在于使用一个轧出或锻出的单件厚板圆盘,先行模锻成球面形状,然后用专用工具冲出接管。这样得
目前,热处理工件变形的校直方法很多。高频热点校直法是一种比较先进的校直方法。尤其是对一些尺寸较大,形状复杂的工件,用其它的方法都难以校直,而采用高频热点校直法均可
Z 41-5型5毫米螺母多工位自动冷镦机,是天津机械配件工业公司包建罗马尼亚—标准件厂选用的设备之一。该机是于一九七二年由济南铸锻机械研究所、天津标准件机床修造厂、天
一、前言金属清洗技术在工艺生产中占有重要地位。长期以来,担当清洗工艺中最普遍、最常用的清洗剂是:汽油、煤油、丙酮等等有机溶剂。这对于能源的浪费、生产的安全、环境
为了加强广大地质学会会员之间的联系,江苏省地质学会试办“地质沙龙”,旨在为会员提供交流学术思想、地质市场信息,加强同行联谊的场所和机会,以期广泛的思想和信息交流有
一、概述 SD 120 F电动磨头(见图1)转速120,000转/分,被用在 MZ 201型全自动小孔内圆磨床上,可以磨削直径1~2毫米的小孔,光洁度 9以上。磨头除定子壳体部分进行冷却外,为了降
大马力履带推土机行走机构在大负荷与承受一定冲击和严重磨损条件下服役,其中销套、链轨节、履带板、支重轮和驱动轮极量损坏。通过攻关,合理的用材、正确的热处理工艺,寿命