Microstructure,mechanical properties and corrosion resistance of as-cast and as-extruded Mg-4 wt% Zn-1 wt% La magnesium alloys were investigated.The alloys were p
Pt-diffused coatings were synthesized on Ni10Al alloy by electroplating a thin layer of Pt (1-5 μm) followed by a diffusion treatment in vacuum at 1000-1100 ℃
The effects of alloying elements (Co,Cr,Mo,W,Al,Ti,and Ta) on the oxidation resistance of Ni-(0-15)Co-(8-15)Cr-(0-5)Mo-(0-10)W-(3-8)Al-(0-5)Ti-(0-10)Ta-0.1C-0.0