冶金部自动化研究所与邯郸钢铁总厂合作进行的焦炭称量控制与水分补正装置于1982年12月13日投入生产试验。试验过程中固定干焦量,每30分钟采集一次焦炭水分值,由水分值装置算出湿焦计算值,据湿焦的计算值人工调整湿焦设定值(因水分湿度仪有问题,装置不能转自动调整),使之和湿焦计算值一致。随焦炭所含水分变化调整湿焦装入量,达到入炉干焦量稳定。经连续80小时的运行(因建防尘室而 Metallurgical Institute of Automation and Handan Iron and Steel Plant in cooperation with the coke weighing control and moisture correction device on December 13, 1982 put into production test. During the test, a fixed amount of dry coke was collected and the coke moisture value was collected every 30 minutes. The calculated value of the wet coke was calculated by the moisture value device. The wet coke set value was manually adjusted according to the calculated value of the wet coke (because of the problem of moisture meter, The device can not be automatically adjusted), so that it is consistent with the calculated value of wet coke. With the coke moisture content changes to adjust the amount of wet coke into the furnace to dry the amount of coke stability. After 80 consecutive hours of operation (due to the construction of the dust chamber
其他文献
一、地質矿床情况我矿为高中溫热液充填,含鎢錫銅等多金属,多次成矿急傾斜薄矿脉的脉状矿床。脉石为乳白色石英脉,比重2.7。围岩全为等粒与中粒花崗岩。围岩蝕变有云英岩化
由于电弧炉加热存在炉温不均的弱点,以及我国普遍存在电力供应不足,炉子电功率不够等,因而单位电耗普遍较高,迫切需要寻找新的途径提高热效率,降低电耗,节约能源。 为此,针对
期刊
食管癌贲门癌切除,因手术的刺激会影响病人的心率,严重者可导致心跳骤停。术前正确判断病人心动过缓的性质,采取相应的处理,是安全度过手术期的重要一环。临床资料本组106例
根据冶金工业部年初发出提高四大指标的号召,經过半年来的努力,各銅矿选厂在提高銅精矿品位方面都取得了很大的成績。銅精矿品位一般从9~10%提高到15~20%;选矿回收率不仅未见
1975年12月,湘钢二号高炉(750米~3)采用了“顶风上料”开炉的方法。1977年10月,一号高炉大修后开炉,再次使用了这个方法,都取得了良好效果。该方法过去在国内仅在某些300米~
典型的腺鳞癌和鳞癌在病理形态上不难辨认,非典型者,尤其是两者混合存在时,HE染色常不易区分。我们根据两者所含物质成分的不同,对6例腺鳞癌标本探讨了用阿尔辛绿和四碘荧光素进
电晕除尘机和分級机的原理是利用在处于强电場作用下的气体(空气)中产生的物理現象。这类选矿机的一部分电极通常是接地式的,由密实的和穿孔的板面制成,而另一部分电极是电
标准和标准化是产品创优工作的重要内容之一。本文讨论了企业标准化的定义和地位;分析了产品创优工作中的标准化活动现状和经验,对进一步健全优质产品标准体系作了具体探讨。
根据我国四个现代化战略目标,今后发展钢铁工业应以老厂改造为主,因之研究老厂的总图运输改造是具有深远意义的。本文试以邯钢总图运输改造为例。探讨一下中型钢铁厂总图运