论文部分内容阅读
以(Ba_(0.6)Sr_(0.4))TiO_3为基料,掺杂半导化元素及添加剂,选用最佳烧结工艺,获得了较好的低居里点(约0℃)缓变型线性化PTCR材料,该材料可用于测温与控温装置。
Based on the Ba_ (0.6) Sr_ (0.4) TiO_3 as the base material, the semiconducting elements and additives were doped, and the best sintering process was chosen to obtain the better slow Curie point (~ 0 ℃) Material, the material can be used for temperature measurement and temperature control device.