基于聚多巴胺的超疏水棉织物的一锅法制备及其油水分离性能

来源 :材料研究学报 | 被引量 : 0次 | 上传用户:YANCONG1103
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
将棉织物浸入多巴胺、硝酸银、十六烷基三甲氧基硅烷的乙醇溶液中,取出烘干制备出超疏水棉织物.用扫描电子显微镜和X射线光电子能谱表征其表面形貌和元素,用接触角测量仪测量其接触角并进行摩擦或液体浸泡(如酸、碱、沸水)实验检测其耐用性.结果 表明,聚多巴胺的强附着性使原位生成的银纳米粒子能经受摩擦或不同液体的浸泡,从而使超疏水织物具有良好的耐用性.超疏水棉织物还具有良好的油水分离性能,其油水分离效率高达97%,油流量最高可达15.93 m3·m-2·h-1.
其他文献
1.IntroductionrnMicro-topology is of fundamental significance to materials,the properties of which are largely correlated with their inner features,be it orientation pattern,grain boundaries and micromorphology,to name a few[1-7].For subtle nano-architect
期刊
For gaining fundamental insight into coating wear mechanisms and increasing operational efficiency and automation degree of equipment in important application fields of coating techniques,it is of great im-portance to developing novel wear measurement tec
Al-Mg-Si alloys (6000 series) exhibit a promising prospect as conductive materials due to their high specific strength,high electrical conductivity,excellent formability,good weldability,cor-rosion resistance and relatively low cost [1-3].These optimum pr
期刊
The continuous growth in the manufacture of aerospace components such as blisks has led to an increase in the application of different hybrid materials fabricating methods,and thus the requirements for join-ing and strengthening of dissimilar welds.Accord
This study focuses on the transient liquid phase (TLP) bonding of DD5 single-crystal superalloy to CrCoNi-based medium-entropy alloy (MEA) using a BNi-2 filler alloy.The microstructure and mechanical proper-ties of the TLP-bonded DD5/MEA joint were evalua
To date,Co-based metal-organic frameworks (Co-MOFs) have drawn much attention owing to their ad-vantages of easy preparation,high porosity and adjustable structure.Because of these enticing properties,numerous efforts have been devoted to their applicatio
The influence of surface roughness on the interfacial dynamic recrystallization kinetics and mechanical properties of Ti-6Al-3Nb-2Zr-1Mo hot-compression bonding joints was systematically investigated.It is found that for the bonding interface of rough sur
Sc solute clusters with a high number density were produced in an Al-0.3 wt.%Sc alloy when aged at 250 ℃,while fine Al3Sc precipitates were predominantly formed in the same alloy aged at 300 ℃.The alloy strengthened by Sc solute clusters displayed higher
用固相反应法制备(Gd1-xEr)2(Zr0.8Ti0.2)2O7(摩尔分数x=0,0.2,0.4)陶瓷并测试其晶体结构、显微形貌和物理性能,研究了Er2O3掺杂的影响.结果 表明,(Gd1-xErx)2(Zr0.8Ti0.2)2O7陶瓷具有立方烧绿石结构,显微结构致密,在室温至1200℃高温相的稳定性良好;Er3+掺杂降低了陶瓷材料的热导率和平均热膨胀系数,当x=0.2时,其1000℃的热导率最低(为1.26 W·m-1 ·k-1).同时,Er3+掺杂还提高了这种材料的硬度和断裂韧性.
The corrosion of unaged and 7000-h thermally aged 308L stainless steel weld metals in simulated PWR primary water under aerated and deaerated conditions was investigated,involving the corrosion of austenite,δ-ferrite and δ-ferrite/austenite phase boundary