对于含有多种金属矿物以及银呈不同形式存在的矿石,由于物理和物理-化学性质上的差异,使含银矿石的选矿问题变得复杂化。 通常,浮选这种矿石是按回收主要金属(有色金属)确定条件。显然,这样选择流程不能保证很好地回收银。 研究结果表明: (1) 矿石氧化较深,2/3的铅矿物呈氧化物形式:铅矾(34%),白铅矿(6.8%),铅铁矾(25.2%)。但是锌矿物氧化程度较低,矿石中90%的锌是闪锌矿; For ores that contain many metallic minerals and different forms of silver, the beneficiation of silver-bearing ores is compounded by the physical and physical-chemical differences. Generally, flotation of such ores is based on the recovery of the major metals (non-ferrous metals). Obviously, such a selection process can not guarantee good recycling of silver. The results show that: (1) Ore is deeply oxidized. Two thirds of the lead minerals are in the form of oxides: lead alum (34%), white lead ore (6.8%) and lead iron alum (25.2%). However, the degree of oxidation of zinc minerals is low, 90% of the zinc in the ore is sphalerite;
其他文献
一、绪言 在连铸中,对影响保护渣的熔化温度,粘度,导热率等物理性质的有关问题进行了很多研究,其各自的适应范围也正在被人们所了解。但是它们购物理性质是互相关联的,难以单
一、前言喷射冶金技术具有设备简单、投资少、上马快、效果显著等优点,当今国内外冶金工作者已将它作为提高钢质量行之有效的一个重要手段。为了改善特殊钢的质量,提高生产
本文研究了硅酸锌矿直接酸浸工艺中的主要技术关键及其解决途径。通过采用控制浸出终酸pH值1~2,温度45~80℃,时间1~2小时,锌离子浓度100~140克/升,SiO_295%,过滤速度1.5~3米~3/米~2
简要总结和分析了包钢3座高炉铁口泄漏煤气处理所采取的基本对策及其效果,并分析了铁口泄漏煤气的原因. This paper briefly summarizes and analyzes the basic countermea
前言经过多年的试验研究和改进,直接还原已经成为一种完备的炼铁方法,图1表示出 Preface After years of experimental research and improvement, direct reduction has b
SL/RN回转窑直接还原工艺可以采用非焦煤。为了改善经济效益,我们对废气余热和残炭的利用进行了研究。最有吸引力的方案是用废气余热来生产蒸汽或发电。余热生产蒸汽的方案已
硫是钢中的有害元素。近代工业的发展,对钢的质量提出了愈来愈高的要求,因此对钢中硫含量的要求也就愈来愈苛刻。而炼钢过程的脱硫能力往往是有限的,一般平炉、转炉的脱硫能
易拉罐—3004H19铝合金板带材主要用于食品饮料包装。因其性能参数要求高,生产工艺极为复杂,不仅在国内是一项空白,国外也只有美国、西德、日本等少数国家能够生产。目前,我