在底漆线的生产过程中,参数的控制尤为重要,每个槽液参数的微小变化,均会引起电泳驾驶室外观质量的变化,在日常的工作中,对底漆线的各种质量问题及参数调整方法进行了总结。1表调加料流程的改进之前,表调剂添加的方式为一次添加,添加后不再进行补加,由于脱脂后表调液的保质期较短,该加料方式无法保证表调液的活性,从而影响驾驶室的表
In the production process of primer line, the control of parameters is especially important. The slight change of each bath parameter will cause the change of appearance quality of electrophoresis cab. In the daily work, the quality problems of primer line And parameter adjustment methods were summarized. Table 1 before the addition process to improve the feed, the table is added to add a modifier, add no longer add, due to the degreasing table liquid shelf life is shorter, the feeding method can not guarantee the activity of the table liquid, thus affecting Cab table