论文部分内容阅读
Polyethylene terephthalate(PET) with molecular formula of(C10H8O4)n foil stacks were irradiated by 25 MeV/u Kr ions in the vacuum chamber 1.33×10-5 Pa at room temperature. The irradiated fluence
Polyethylene terephthalate (PET) with molecular formula (C10H8O4) n foil stacks were irradiated by 25 MeV / u Kr ions in the vacuum chamber 1.33 × 10-5 Pa at room temperature. The irradiated fluence