采用选择性絮凝脱泥,阴离子反浮选工艺流程选别美国蒂尔登铁矿石获得良好结果。铁精矿含磷降至0.030%以下,铁精矿品位65.5%,回收率79.67%。
Using selective flocculation desliming, anion reverse flotation process selected the United States Tielon iron ore to obtain good results. Iron ore concentrate reduced phosphorus below 0.030%, iron concentrate grade 65.5%, recovery rate of 79.67%.