【摘 要】
:
1980年年中,我们决定在密苏里州,新马德里诺兰达铝业公司铝电解厂建第三电解槽系列和阳极焙烧炉。对新阳极焙烧炉的主要技术要求如下:1.焙烧阳极能力为5.5万吨/年;与现有两
论文部分内容阅读
1980年年中,我们决定在密苏里州,新马德里诺兰达铝业公司铝电解厂建第三电解槽系列和阳极焙烧炉。对新阳极焙烧炉的主要技术要求如下:1.焙烧阳极能力为5.5万吨/年;与现有两座焙烧炉的每座产能相比约增加20%;2.该炉必须控制在有限的有效空间范围之内,该空间三面紧靠现有的两座焙烧炉和阳极贮存室;3.消除由于现有两座地下焙烧炉引起的
In mid-1980, we decided to build the Third Electrolytic Cell Series and the anode roaster at the Aluminum Electrolysis Plant in Nolande, Missouri, New Madrid. The main technical requirements for the new anode roaster are as follows: 1. The anode capacity for roasting is 55,000 t / y, an increase of about 20% compared to the capacity of each of the existing two roasters; 2. The furnace must be controlled at a limited Within the effective space, the space on three sides close to the existing two roaster and anode storage room; 3. Elimination due to the existing two underground roaster caused
其他文献
传统的高炉炼铁法是一项复杂而庞大的生产工艺。从矿石到生铁要经过许多生产环节,原燃料经过反复加热、冷却和加工,大大提高了产品的成本和能耗。办了改变这一现状,炼铁工作
本文着重介绍了攀钢转炉炉龄试验及生产结果。由于确立了炼钢新渣系及适宜的冶炼工艺操作,创造出同类转炉炉龄711炉的先进水平。
This article focuses on the Panzhihua co
从高炉冶炼发展趋势出发,为提高副产品的应用价值及强化高炉生产过程、分析了煤气脱除 CO_2的意义和经济效果。按当前鞍钢高炉煤气组成,脱除 CO_2为30%,并以此加入高炉鼓风中
在采用成分稳定、理化性能较好的原燃料的前提下,十、十一高炉进行正分装大批重试验,提高了顺行压差,炉料透气性改善,炉况顺行变好;冶炼过程中选择合理的造渣制度;严格控制
一、生产情况 中国钨矿资源十分丰富,是世界上储量最大、产量最多的国家。现有40多个国营矿山和近200个矿点、42个重选厂和2个4000吨以上的精选厂在生产。生产能力逐步扩大,
本文研究了钯的加入量、烧结温度和烧结时间对钼的密度的影响。实验结果表明,钯的最适宜的加入量为0.5wt%左右。在这个最佳量下钼的最适宜的烧结温度为1150℃。利用实验数据计
机械工业部通用基础件局于一九八五年五月二十七日至二十九日在宁波粉末冶金厂主持召开了“氮基气氛在粉末冶金铁基零件烧结中应用”鉴定会。氮基烧结气氛作为粉末冶金铁基
冶山铁矿选矿厂1972年投产以来,选铜技术指标一直较低,1978年~1981年平均指标仅达到:铜精矿品位12.58%,铜实际回收率48.16%。生产实践表明,采用浮选柱作为铜钴混合浮选设备,不
杭钢8米~2竖炉球团造球工艺中(φ4.2米圆盘造球机),1984年9月在给水管路上,安装了广东省钢铁研究所研制的HCM强磁除垢器,磁化造球过程中添加的补充水,经两个多月来的使用,效
一、为什么要炉底出钢?有两个主要原因促使炉底出钢的开发其一:为了提高钢的质量,很多国家确定了电弧炉-钢包炉工艺,此工艺要求电弧炉能提供“无渣钢水”,各国在这方面曾做