病虫害发生规律研究与绿色防控

来源 :中国烟草学会2018年学术年会 | 被引量 : 0次 | 上传用户:zzp90518
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
  Green peach aphid [Myzus persicae(Sulzer)] and tobacco mosaic virus are the primary causes of disease in flue-cured tobacco in China and in many other regions of the world.Control of tobacco diseases and pests relies primarily on chemical agents.However,serious problems related to chemical control have emerged.A field experiment was conducted to determine the effects of genetic diversity on pest and disease control in a tobacco ecosystem.In 2012 and 2013,the Minyan 38 and K326 flue-cured tobacco varieties were intercropped in Wuping County,in Longyan City in Fujian Province,P.R.China.Tobacco disease caused by green peach aphid and tobacco mosaic virus was significantly affected by the intercrop system.The green peach aphid density,tobacco mosaic incidence rate and disease severity index decreased by 60.61%,34.76%and 0.05,respectively,in 2012 and by 61.89%,23.51%and 0.01,respectively,in 2013 in the intercropped fields relative to monoculture stands.The tobacco yield and monetary value of the tobacco leaves increased from 0.81%to 0.98%and from 1.15%to 2.45%,respectively,with intercropping.The serious problems associated with control of this pest and the virus diseases it vectors might be avoided using this approach and consequently a greener protection of tobacco may well be realized.
其他文献
The feasibility of measuring the low concentrations of phenolic and amine antioxidants in ester oils has been researched by using near-infrared and mid-infrared spectroscopy. The phenolic antioxidant
WC based coatings deposited by high velocity oxy-fuel spraying (HVOF) have been widely used in many fields which are subjected to severe abrasive wear, such as shipping, metallurgy, energy source, and
使用多弧离子镀膜在硬质合金表面镀TiN、TiAlN、TiAlSiN,使用扫描电子显微镜及X射线衍射仪对比研究三种涂层在相同氧化环境下微观形貌和物相组成.实验结果表明:TiN涂层在600℃开始氧化,800℃时涂层表面氧化程度严重;TiAlN涂层在700℃开始氧化,800℃时有少量的Al2O3生成;TiAlSiN涂层在800℃时无明显氧化现象.三种涂层的抗氧化性能呈现如下关系:TiAlSiN>TiAl
铝合金车身覆盖件已经成为解决汽车轻量化问题的关键技术途径之一。但铝合金冲压成型的性能较差,加之冲压工艺过程包含复杂的物理现象,使得铝合金冲压成型件易形成拉裂,起皱和回弹等缺陷。铝合金冲压成型工艺过程的复杂性使得对其设计和控制变得非常困难,是制约车用铝合金覆盖件发展和应用的技术瓶颈之一。现阶段或用计算机仿真分析理论铝合金成型性能,或在模具调试阶段弥补例如回弹补偿量的不足,消除起皱,预防拉裂等成型缺陷
会议
三元硼化物金属基陶瓷Mo2NiB2具有优良的耐磨、耐蚀性能,其作为涂层在海洋防腐中有广泛的应用,如船舶、海洋管道、海洋平台、海港设施等的防腐.激光熔覆原位合成法是一种在碳钢表面制备三元硼化物涂层的新型方法.原位反应是利用不同元素在一定条件下发生化学反应,在金属基体内形成一种或多种增强相.激光熔覆原位合成法是利用激光高能作为固-固原位反应激发条件,在金属基表面形成超细增强陶瓷相.本文利用激光熔覆原位
汽轮机隔板为高温高压蒸汽导流部件,汽轮机隔板通流部分表面粗糙增大会导致汽轮机通流部分性能退化,使汽轮机组的功率和效率降低,热耗率增加。合适的喷丸参数能保证处理表面粗糙度,同时有利于提高处理表面清洁度。试验研究了不同粒径、硬度钢丸及不同喷丸参数对试样表面粗糙度、喷丸效率等的影响规律。研究表面,喷完后试样表面粗糙度随着喷丸钢丸直径增大、钢丸硬度增加而增大,但是钢丸直径减小、硬度降低会导致喷丸效率降低。
金属塑性拉延成形应用广泛,但塑性成形界面的接触压力和摩擦温度往往较高,在某些严酷工况环境下,传统油脂无法实现有效地润滑,而固体粉末润滑对极端工况具有良好适应性。爬行现象在工程实践中较普遍,在基于粉末润滑的拉延成形中,其直接体现是试件表面粉末边界层上形成纵向的压痕或划痕,从而造成润滑膜的破坏。因此研究金属塑性成形过程中爬行现象,对维持机器设备运动的连续性,提高加工零件的表面质量以及粉末润滑的推广都具
颗粒流润滑是利用大量松散的固体颗粒在界面中的承载和剪切行为实现特殊环境下界面的减摩,在高温成形制造等领域得到广泛应用,因此研究颗粒介质摩擦界面在剪切过程中的受力情况,对颗粒流润滑机理的分析以及润滑装置的设计都具有重要的意义。研究中将第三体颗粒类比为流体,基于雷诺方程、粘度方程、G-W模型等建立含大颗粒粗糙界面的三体接触模型。该模型中摩擦副的总载荷W由流体承载WL、微凸体承载WG和大颗粒承载Wk共同